When pump fluid goes wrong, the signals on the floor are vague: the gauge creeps upward, a haze appears on workpieces, the pump sounds muffled, the oil window darkens day by day. Behind any of these may sit a wrong grade, a cold trap left off, a weakening backing pump, or fluid that has thermally aged. This article takes six common vacuum duties and puts grade matching, change intervals and fault diagnosis together into a sequence that can be run on site.
| Duty | Vacuum requirement | Grade | Point to watch |
|---|---|---|---|
| Vacuum coating | 10⁻⁴–10⁻⁵ Pa band | 702 or 704 | Backstreaming contamination of the deposited film |
| Optical coating | 10⁻⁴ Pa band | 704 | Film uniformity is sensitive to oil vapour |
| Semiconductor and e-beam equipment | 10⁻⁵ Pa band and deeper | 704 or 705 | Cleanliness takes priority; assess the cold trap |
| Electron microscopy and mass spectrometry | 10⁻⁷ Pa band and deeper | 705 | Cold trap recommended to cut background interference |
| Vacuum melting and furnaces | 10⁻³–10⁻⁶ Pa band | 702 or 704 | Metal vapour and dust accelerate fluid degradation |
| Tubes, lamps and displays | 10⁻³–10⁻⁵ Pa band | 702 | Throughput takes priority, with cost kept in view |
One clarification: the table states vacuum in Pa while fluid parameters are quoted in torr, and 1 torr ≈ 133.3 Pa. Convert to one unit when writing a scheme, otherwise a comparison can misread three orders of magnitude as none.
Change intervals are not fixed values; boiler temperature, the gases being pumped and system cleanliness all move them. Practice is to change on signal rather than by calendar.
| Duty | Reference interval | Main degradation driver |
|---|---|---|
| Vacuum coating | 12–18 months | Re-deposited coating vapour, frequent chamber opening |
| Semiconductor equipment | 18–24 months | High cleanliness demand, low tolerance for degradation |
| Optical coating | 12–18 months | Film quality is sensitive to oil vapour |
| Research instruments (EM, MS) | 18–24 months | Low tolerance for background interference |
| Vacuum furnaces and melting | 6–12 months | Metal dust, radiant heat, oxides |
Those intervals are engineering references. The vacuum decay curve and fluid test results govern in practice.
| Symptom | Suspect | Check | Action |
|---|---|---|---|
| Vacuum falls slowly | Thermal ageing or light-fraction build-up | Colour, viscosity, vapour pressure; boiler temperature too high | Change fluid and re-check the temperature set point |
| Vacuum drops suddenly | Leak rate, failed cold trap, weak backing pump | Leak-check in sections; check trap level; measure backing vacuum ceiling | Repair the structure; changing fluid rarely helps |
| Haze on workpieces | Backstreaming of oil vapour | Baffle and trap condition; boiler temperature | Fit or clean baffle and trap |
| Slow start, muffled sound | Viscosity too high, or low fluid level | Level; wrong grade fitted | Top up, or return to the correct grade |
| Rapid darkening, coked jets | Oxidation or contamination | Frequent venting; oxygen in process gas | Shorten the interval, consider sealed operation |
The key is separating fluid problems from system problems. A simple method: run a known-good fluid of the same grade as a control. If vacuum does not improve, the fluid was not the cause.
Diffusion pumps run at boiler temperature, and viscosity moves with temperature, which affects start-up and jet stability.
| Kinematic viscosity (25°C, mm²/s) | Viscosity–temperature coefficient | Melting or pour point (°C) | Flash point (°C) |
|---|---|---|---|
| 0.65 | 0.32 | −68 | not stated |
| 20 | 0.59 | −84 | 232 |
| 50 | 0.59 | −70 | 285 |
| 350 | 0.60 | −65 | 315 |
| 1,000 | 0.61 | −50 | 315 |
| 10,000 | 0.61 | −48 | 315 |
| 100,000 | 0.62 | −41 | 321 |
Three conclusions apply directly on site. Heavier grades carry larger coefficients, so cold start-up in winter and sagging in summer heat both worsen with viscosity. Flash point rises with viscosity yet remains a safety figure, not a statement of long-term heat tolerance. And pour point climbs with viscosity, so a pump shut down in a northern winter needs pre-heating before restart.
IOTA publishes a viscosity–temperature coefficient range of 0.31–0.61 for its dimethyl series, consistent with its graded property data.
| Direction | Feasible | What to check at the same time |
|---|---|---|
| 702 to 704 | yes, deeper vacuum | Start-up takes longer and throughput falls; confirm the process accepts it |
| 704 to 705 | conditionally | Cold trap needed; boiler temperature and flash margin re-checked |
| 705 to 704 | a downgrade in practice | Design vacuum will not be met; assess the process floor |
| Mixing grades | not advised | Vapour pressure becomes unpredictable and refractive index cannot reveal the ratio |
The test for substitution is not whether the fluid fits in the pump, but whether the system still meets its original vacuum at its original tempo.
Rule out leaks, the cold trap and the backing pump to begin with. A same-grade control fluid locates the fault quickly.
Stepping up costs slower start-up and higher pumping resistance. Where the process does not need the extra depth, that is over-specification.
torr and Pa differ by roughly 133 times; mixing them in a scheme misplaces the grade outright.
Degradation speed varies widely between processes, so changing on signal is both cheaper and safer.
Old and new fluid mixed together have unpredictable vapour pressure, and coke deposits block the jets.
It follows from the vacuum requirement. The 10⁻⁴–10⁻⁵ Pa band is served by 702; where film cleanliness matters and the 10⁻⁷ torr region is needed, choose 704.
Because background gas interferes visibly with imaging and analysis. At about 3×10⁻¹⁰ torr, 705 with a cold trap holds residual gas very low.
No. Coating duties commonly run 12–18 months, semiconductor and research instruments 18–24 months, furnaces and melting 6–12 months, adjusted by vacuum decay and fluid testing.
Leaks and the cold trap to begin with, then the backing pump. Changing fluid does not fix structural problems, and a same-grade control fluid is the quicker way to tell.
Viscosity rises as temperature falls, and heavier grades rise more. Pre-heat pump body and fluid so the jet is stable and start-up is not laboured.
Not advised. Vapour pressure becomes unpredictable and refractive index cannot reveal the mixing ratio. Drain and clean pump body and jets when switching.
Company note: Iota Silicone Oil (Anhui) Co., Ltd., based in Bengbu, Anhui, covers diffusion pump fluid grades 702, 704 and 705 alongside phenyl fluids, methyl fluids, hydrogen fluids, hydroxyl fluids, vinyl fluids, silanes, fumed silica and platinum catalysts, supporting vacuum coating, semiconductor, research instrument and vacuum melting customers with selection guidance and on-site support.